Bead Blasted Titanium Plate
Sunrui Titanium Bead Blasted Titanium Plate is a precision finished titanium flat material produced by skilled bead peening treatment. We use high speed spherical media such as glass, ceramic and zirconia beads to evenly treat the titanium substrate surface, successfully erasing rolling lines, machining burrs and high temperature heat tint. The technique results in a homogeneous non-directional matte satin texture. The procedure results in uniform surface compressive residual stress, which considerably improves material fatigue strength and stress corrosion cracking resistance. Backed by more than 60 years of professional titanium production expertise, we produce customized bead blasted titanium in hot rolled (2.5~60 mm) and cold rolled (0.4~4.0 mm) standards, with max width up to 2500 mm and length up to 8000 mm to satisfy various precision industrial requirements.
The conventional mill-finished titanium plates include direction rolling markings, micro surface flaws and imbalanced residual stress, which are easy to impair the following processing performance and service stability. The bead blasting, which is an effective one-step surface strengthening procedure, may address the above concerns completely.
Meanwhile, the compressive stress layer produced in blasting is equal to expert shot peening strengthening. It can effectively control the growth of micro-cracks in high-cycle fatigue and corrosive conditions, which is an important performance benefit for components in high-standard aerospace and marine equipment.
| Parameter | Details |
|---|---|
| Forged Slab | (70~300) × 1400 × 10000 mm |
| EB Ingot | 200 × 1290/1090 × (1000~6200) mm |
| Hot Rolled Plate | (2.5~60) × (600~2500) × (1000~8000) mm |
| Cold Rolled Plate | (0.4~4.0) × (600~2500) × (1000~4000) mm |
| Hot Rolled Coil | (3.0~12) × (1000~1500) mm, max coil weight 7 ton |
| Cold Rolled Coil | (0.4~4.0) × (1000~1500) mm, max coil weight 6 ton |
| Material Grades | GR1, GR2, GR3, GR4, GR5, GR6, GR7, GR9 (AB-5), GR12, Ti-811, Ti-15333, SP-700, Ti-6242, etc. |
| Standards | GB, GJB, ASTM, ASME, AMS, DIN, JIS, and enterprise standards |
Bead Blasted Titanium Plate retains the good intrinsic capabilities of titanium materials, with additional enhanced surface performance to fit to high-demand industrial scenarios:
High Strength-to-Weight Ratio: Lightweight texture, steady structural strength and efficient lightweight design of precision structural elements.
Corrosion Resistance: Natural titanium oxide layer is resistant to seawater, acidic media and different hostile chemical conditions to provide long-term stable service.
Processability: Applicable to normal titanium welding, bending and mechanical processing techniques, no specific processing threshold.
Thermal Stability: Keeps structural performance stability under high temperature circumstances and long term mechanical cyclic stress.
Biocompatibility: Safe and to come in close touch with human tissue and completely qualified for medical implant applications.
Its bead blasted finish eliminates the surface impurities efficiently, promotes surface activity and offers optimal surface conditions for further painting, anodizing and precise processing.
Biomedical Implants
Titanium plates that have been bead blasted are often utilized in orthopedic trauma plates and implant devices. Controlled uniform surface roughness increases bone osseointegration, minimizes the likelihood of implant rejection and enhances the long-term stability of clinical use.
Aerospace Structural Panel
Applied to aircraft fuselage components and engine heat shields, the non-reflective matte coating prevents interference with airborne optical sensors. The surface compressive stress layer inhibits micro-crack propagation under high vibration and fatigue conditions and effectively prolongs the service life of the component.
Architecture and Home Electronics
The homogeneous satin texture has the anti-fingerprint and scratch concealing effect and is extensively utilized in the shells of high-end electronic equipment, watch accessories and architectural ornamental panels. The blasted surface is also a great substrate for matte anodizing and DLC coating treatment.
Marine & Industrial uses
The completed plate is free from surface iron contamination and residual impurities, which along with titanium’s inherent corrosion resistance, offer low-maintenance and long-life performance in maritime and severe industrial corrosive environments.

Sunrui implements strict full-batch quality inspection for all bead blasted titanium plates to ensure stable and consistent finished quality.
Surface Roughness Testing: Contact and optical profilometers are adopted to detect Ra and Rz values, ensuring uniform surface roughness of each batch of products.
Surface Contamination Inspection: SEM and EDS analysis verify no embedded glass or ceramic media residues, avoiding galvanic corrosion and biocompatibility failures, especially critical for medical-grade products.
Color Uniformity Detection: Spectrophotometer calibration ensures consistent surface matte color, meeting the appearance requirements of architectural and consumer electronic products.
Passivation Performance Verification: Water break test and copper sulfate test confirm the integrity of the surface anti-corrosion oxide film after blasting treatment.
We exclusively adopt stainless steel and ceramic blasting media, completely avoiding carbon steel media that causes iron contamination. Regular media screening and cycle testing ensure stable blasting particle shape and consistent finished surface quality.

Q1: Will bead blasting change the dimensional tolerance of titanium plates?
A: Bead blasting only acts on the micron-level surface layer with negligible material removal. For ultra-thin plates, we will conduct dimensional calibration to eliminate minor surface tension deformation and ensure standard dimensional accuracy.
Q2: Is blasting available for thin titanium plates below 1mm?
A: Single-sided high-pressure blasting may cause plate warping. We recommend double-sided synchronous blasting or low-pressure wet blasting for thin-gauge plates to effectively control stress deformation.
Q3: Does bead blasting affect titanium's corrosion resistance?
A: Qualified blasting treatment will not reduce corrosion resistance. We use special non-ferrous blasting media to avoid iron contamination and surface defects, retaining the titanium's original anti-corrosion performance.
Q4: Can the products be anodized?
A: Yes. The uniform matte surface is an ideal pre-treatment base for Type II and Type III anodizing, featuring strong oxide layer adhesion and stable non-reflective coloring effect.
Q5: Is the bead blasted surface finish durable?
A: The surface texture is formed by physical shaping, no peeling or fading occurs in daily use. It can only be changed by strong mechanical grinding.
Q6: How to solve fingerprint contamination on matte surfaces?
A: For consumer-grade products, post-blast anodizing or AFP nano anti-fingerprint coating can be customized to seal the surface texture and improve stain resistance.

If you are in need of high-precision, stable-performance Bead Blasted Titanium Plate for medical, aerospace, electronic and marine projects, please get in touch with our professional team via srt@sunrui-ti.com.